Prusament ABS: Practical Tips for Warp-Free Prints
To avoid warpage, use a brim with 8mm width, 0.2mm separation, first layer fan off, ramp to 30%. Bed temp 110°C on PEI with ABS slurry, chamber temp min 45°C. Dry at 80°C for 4 hours.
By Lucas Fuentes

ABS FilamentPros & Cons
Flashforge ABS Filament Buying Guide
Flashforge ABS offers consistent diameter tolerance (±0.02 mm) and low warpage for functional prototypes and jigs. Requires heated chamber above 50°C, 245°C nozzle, 100°C bed. Best for job shops and production lines.